Corrosion investigations were carried out on samples, which were stored for up to 28,500 hours in the stack gas of the VOeRDE powerstation in the temperature range of 720 C to 905 C. There is some weakening of the material, which is determined by internal oxidation (Incoloy 800H, 2.4663, Thermon) and metal removal. For AC66, there was no internal o...
Germany
Germany
Germany
Germany
Germany
The content of natural radionuclides in coal and in the residual materials after burning was investigated. Special caution is necessary in handling this dusty residual material with regard to radiation exposure by the pathway of inhalation. The processing of such material in concrete and other construction materials is not relevant for radiation ex...
According to indications of the working group for questions on the climate of the association of German electric utilities (VDEW), energy application of power generation contributes to the German CO_2-emission with about 30%. A reduction of CO_2-emissions in electro-economics can be achieved especially with a decrease of the application of fossil e...