Affordable Access

Adaption of remelting procedures for the use of recycled metal in nickel-base superalloy castings

Authors
Publication Date
Source
OpenGrey Repository
Keywords
  • 13H - Industrial Processes, Manufacturing Processes
External links

Abstract

Statistics