Austenitic Superheater Materials - Steamside oxidation and flue gas corrosion after 23000 hours service at Vestkraft coal-fired power station

Publication Date


The corrosion behaviour, both on the fireside and steamside of various austenitic steels was investigated. This was undertaken by exposure in the test superheater loop at Vestkraft