Abstract

Abstract Fe-21Mn-2.5Al-0.04C alloy was exposed to SO 2-O 2 mixed gas environments at 900°C. The morphologies of the scales formed on the alloy investigated were examined by scanning electron microscopy and x-ray mapping techniques. The results showed that multilayered scales were formed, consisting of an external (FeMn) 2O 3 blocky oxide, an intermediate (FeMn) 2O 3 internal oxide, and an innermost Mn(Fe)S sulfide.

There are no comments yet on this publication. Be the first to share your thoughts.

Statistics

Seen <100 times
0 Comments

More articles like this

Microstructure of Steel 5Cr21Mn9Ni4N Alloyed by Ra...

on Journal of Iron and Steel Rese... Jan 01, 2006

Aqueous corrosion properties of austenitic Fe-8.7A...

on Surface and Coatings Technolog... Jan 01, 1986

On the low-cycle fatigue response of pre-strained...

on International Journal of Fatig...

Effect of Nb and Mo on the hot ductility behavior...

on Materials Science and Engineer... Oct 20, 2014
More articles like this..