Ren, Wei Lan, Xi Guo, Zhancheng
Published in
Journal of The Electrochemical Society
In this study, pulse reverse current electrodeposition was employed to fabricate Fe-55 wt%Ni alloy. Abnormal grain growth induced by the precipitation of second-phase particles during annealing resulted in a coarse-grained electrodeposited Fe-55 wt%Ni alloy. The grain evolution process during annealing was investigated, and the temperature for abno...
Wang, Qinghao Cui, Ye Li, Xinghao Wu, Pulin Wang, Haosheng Zhang, Zhongwu
Published in
Smart Materials and Structures
In this paper, the effects of Ti content on the solvus temperature of γ-phase and abnormal grain growth (AGG) in Fe43.5−x Mn34Al15Ni7.5Ti x (x = 0, 0.5, 1 and 1.5) shape memory alloys (SMAs) were investigated. It is found that, the increase of Ti content leads to a significant reduction of the solvus temperature of γ-phase, a significant refinement...
Krill, Carl E. III Holm, Elizabeth A. Dake, Jules M. Cohn, Ryan Holíková, Karolína Andorfer, Fabian
If variety is the spice of life, then abnormal grain growth (AGG) may be the materials processing equivalent of sriracha sauce. Abnormally growing grains can be prismatic, dendritic, or practically any shape in between. When they grow at least an order of magnitude larger than their neighbors in the matrix—a state we call extreme AGG—we can examine...
Li, Jina Su, Jie Liu, Geng Ding, Yali Wang, Ao Yu, Linran
Published in
Materials Research Express
In this study, systematic heat treatment routes including solution (980 °C to 1130 °C) and aging (675 °C to 775 °C) processes were used to tailor the microstructural evolution and mechanical performance of a Fe-Ni-Cr based austenitic alloy, strengthened by a γ′ phase (Ni3(Ti, Al)). Grain growth was observed with increasing solution treatment temper...
Qin, Dongyang Liu, Huifang Li, Yulong
Published in
Materials
In order to fabricate homogeneous large-scale Ti-5Al-5V-5Mo-3Cr (Ti-5553) alloy bulk with fine and equiaxial β grain, we performed a series of multi-axial α + β field forging with 62 forging cycles on the large-scale Ti-5553 billet by using 12.5 MN high-speed hydraulic press. The β-annealed microstructure was the starting microstructure of the bill...
zhang;, ju hongfang
0.9KNbO3-0.1BaTiO3 ceramics, with a bimodal grain size distribution and typical tetragonal perovskite structure at room temperature, were prepared by using an induced abnormal grain growth (IAGG) method at a relatively low sintering temperature. In this bimodal grain size distribution structure, the extra-large grains (~10–50 μm) were evolved from ...
Morimoto, Takaaki Shimono, Seiya Yoshiichi, Yuto Kishimura, Hiroaki Ishii, Keisuke
Published in
Japanese Journal of Applied Physics
We investigated the effects of 0.5 mol% to 6.0 mol% CuO addition on crystal growth by the rapid solid-state crystal growth method to synthesize large unitary rectangular (K,Na)NbO3 (KNN) single crystals several square centimeters within 24 h. X-ray photoelectron spectroscopy and X-ray powder diffraction measurements revealed that CuO and Cu2O segre...
jiao;, xueyan
The microstructure evolution and grain growth kinetics of the fine-grained extruded Mg-Nd-Zn-Zr alloy were investigated by holding the extruded plate for a wide range of time in the temperature range of 470 °C to 530 °C. By observing the optical micrographs, it was found that the material showed abnormal grain growth at the experimental condition o...
park;, yeon-ju
This study investigated the causes of microstructural changes and the resultant electrical properties according to the sintering temperature of 0.96(K0.46−xNa0.54−x)Nb0.95Sb0.05O3-0.04Bi0.5(Na0.82K0.18)0.5ZrO3 lead-free ceramics by analyzing the correlation between vacancy concentrations and 2D nucleation. When sintered for 4 h, no grain growth occ...
xu;, yu an maofeng
In this study, the grain growth behaviour of ZnO-V2O5-based ceramics with 0.25–0.75 mol% additions of PrMnO3 was systematically investigated during sintering from 850 °C to 925 °C. with the aim to control the ZnO grain size for their application as varistors. It was found that with the increased addition of PrMnO3, in addition to the decrease in th...